Created by Glazy Admin 2015-07-16 06:59:40, updated 2015-08-09 13:24:21

Parent: None

Type: Colorant

Weight: 79.5400
Formula Weight: 79.5454
LOI: 35.6200
Thermal Expansion: 0.0000
Oxide CuO
% Analysis 64.38
Formula 1.000

Copper carbonate supplies CuO.
A colorant and flux.
Copper carbonate comes in various shades of green, reflecting
various degrees of hydration. Pure copper carbonate (CuCO3) is
about 64% CuO, whereas the basic carbonate (CuCO3 Cu(OH)2) is
nearly 72% CuO. The basic carbonate is (in theory) easier to
disperse in glazes due to its greater affinity for water.
Prepared from Malachite (CuCO3 Cu(OH)2) and Azurite (2CuCO3
Cu(OH)2) or by chemical processes.
Analyses:
Hopper:
CuCO3
Cooper & Royle:
CuCO3
Rhodes:
CuCO3
Chappell:
CuCO3
Cushing:
CuCO3
Memmott:
CuCO3
Parmelee:
CuCO3
Hamer:
CuCO3
CuCO3 Cu(OH)2 (Copper carbonate basic)
IMC:
CuCO3
CuCO3 Cu(OH)2 (Copper carbonate basic)

Hazards

09/2016 Note: This is a new feature. If there is no safety information below, then that material's data has not yet been added. Some materials only have GHS ratings, while others only have HMIS ratings. Warnings differ between systems and countries. Glazy does not take any responsibility for accuracy of linked SDS information. Contact your ceramics supplier for safety information for your specific materials.
Globally Harmonized System (GHS) Hazardous Materials Identification System (HMIS) SDS Link
Pictograms Signal Word Hazard Statements Health Flammability Hazard Protection
Harmful WARNING Harmful if swallowed.
Causes skin irritation.
Causes serious eye irritation.

Recipes using this material

Name Amount of Copper Carbonate Temp. Atmospheres Surface Transparency Si:Al R20:RO Author
Toms Snowflake 0.2 Δ6 - 7 Oxidation
Semi-glossy Translucent 4.86 0.67 : 0.33 Tom Demeranville
Reynold's Rap 12 Δ08 - 04 Raku
12.81 0.17 : 0.83 Ceramic Recipes
DragonFly 6 Δ06 - 04 Raku
17.93 0.17 : 0.83 Ceramic Recipes
Early Spring Green 2 Δ5½ - 7 Neutral
Glossy Translucent 9.31 0.2 : 0.8 Arline Edmonds
Toms turquoise matte 4.65 Δ6 - 7 Oxidation
Satin-matte Opaque 4.9 0.33 : 0.67 Tom Demeranville
Pinnell Seafoam (toms gb variation) 5 Δ6 Oxidation
Matte 5.14 0.32 : 0.68 Tom Demeranville
Carmen's Turquoise (tom's add more clay variation) 4.3 Δ6 - 7 Oxidation
Satin 4.79 0.33 : 0.67 Tom Demeranville
Splotchy Lavender Cone 10 0.6 Δ9 - 10 Oxidation
Reduction
4.65 0.28 : 0.72 Clemson University---Ceramic Dept.
Purple Haze 1.1 Δ10 Reduction
Satin Opaque 10.14 0.25 : 0.75 Glazy Admin
Sue's Matte Turquoise -new (Cedar Hill) 3 Δ6 Oxidation
Matte Opaque 4.79 0.3 : 0.7 Sue McLeod
Matte Turquoise -old (Cedar Hill) 3.5 Δ6 Oxidation
Matte Opaque 5.1 0.53 : 0.47 Sue McLeod
Sue's SJC -new (Cedar Hill) 3 Δ6 Oxidation
Reduction
Glossy Semi-opaque 8.59 0.5 : 0.5 Sue McLeod
SJC -old (Cedar Hill) 3 Δ6 Oxidation
Reduction
Glossy Translucent 8.95 0.6 : 0.4 Sue McLeod
SM Oribe 5 Δ9 - 11 Reduction
Salt & Soda
Wood
Glossy 9.03 0.12 : 0.88 Christopher Lee
Currie Blue 4 Δ5 - 7 Oxidation
Neutral
Satin-matte Opaque 4.94 0.47 : 0.53 Tamas Ferencz
Turquoise Matte 3.5 Δ4 - 7 Oxidation
Matte Opaque 5.19 0.53 : 0.47 Matt Garrett
Red Green 4.8 Δ6 Oxidation
Transparent 4.24 0.52 : 0.48 Ceramic Recipes
WWW 332 3 Δ6 Oxidation
Matte Opaque 5.18 0.52 : 0.48 Daniel Spruyt
Chance's Opal 4.5 Δ10 Oxidation
Reduction
Glossy Translucent 8.05 0.14 : 0.86 chance taylor
Fake Old Chinese Celadon 1 Δ5 - 6 Oxidation
Neutral
Satin-matte Semi-opaque 5.73 0.27 : 0.73 Tamas Ferencz
John's Red 0.75 Δ5 Reduction
Semi-glossy Semi-opaque 12.7 0.26 : 0.74 Clara Giorello
Copper Blue Green- Original 3 Δ5 - 6 Oxidation
Neutral
Matte Opaque 5.1 0.56 : 0.44 Terry Gess
Rainbow Sand 5 Δ010 - 04 Raku
Matte Opaque 9.65 0.16 : 0.84 Sid Henderson
Egyptian Blue Raku 4 Δ08 - 05 Raku
Glossy Translucent 7.37 0.23 : 0.77 Sid Henderson
Strontium Wheathered Copper 3 Δ10 - 12 Oxidation
Reduction
Semi-matte Opaque 4.76 0.42 : 0.58 chance taylor
pete's cranberry 0.3 Δ10 - 12 Reduction
Glossy Translucent 7.55 0.42 : 0.58 chance taylor
Fish Guts 1 Δ9 - 10 Reduction
Glossy Opaque 9.96 0.22 : 0.78 Sid Henderson
AC Green Suede cone 6 ox. 3 Δ6 Oxidation
4.39 0.2 : 0.8 Alisa Liskin Clausen
Malachite (Silverman) 3 Δ9 - 10 Oxidation
Neutral
Reduction
6.88 0.48 : 0.52 Sid Henderson
Strontium Blue 3 Δ6 Matte 4.8 0.45 : 0.55 Glazy Admin
Wood's Transparent Ice Blue -- Cone 04 0.4 Δ05 - 04 Oxidation
Glossy Transparent 7.11 0.44 : 0.56 Clemson University---Ceramic Dept.
Lisa Orr's Turquoise Cone--04 Glaze 7 Δ05 - 04 Oxidation
14.8 0.75 : 0.25 Clemson University---Ceramic Dept.
Yellow Salt Green Mint High Fire Glaze Base 0.75 Δ9 - 10 Oxidation
Reduction
Salt & Soda
Wood
4.8 0.37 : 0.63 Clemson University---Ceramic Dept.
Val's Turquoise 3134 3 Δ5 - 6 Oxidation
Satin Opaque 14.97 0.3 : 0.7 Clara Giorello
Variegated Slate Blue 3 Δ6 Oxidation
Glossy Translucent 6.39 0.09 : 0.91 Joe Thompson
Sam Chung Satin High Fire Glaze Base 0.5 Δ9 - 10 Oxidation
Reduction
Salt & Soda
Wood
Satin 4.05 0.27 : 0.73 Clemson University---Ceramic Dept.
Yellow Salt Medium Green High Fire Glaze Base 3 Δ9 - 10 Oxidation
Reduction
Salt & Soda
Wood
4.8 0.37 : 0.63 Clemson University---Ceramic Dept.
Shaner's Oribe High Fire Glaze Base 5.49 Δ9 - 10 Oxidation
Reduction
Salt & Soda
Wood
Glossy 9.41 0.14 : 0.86 Clemson University---Ceramic Dept.
Panama Red High Fire Glaze Base 1.99 Δ9 - 10 Oxidation
Reduction
Salt & Soda
Wood
Glossy 9.62 0.26 : 0.74 Clemson University---Ceramic Dept.
MSU Copper Red 0.5 Δ9 Reduction
Glossy Opaque 10.58 0.33 : 0.67 Morehead State University