Created by Glazy Admin 2015-07-16 06:59:40, updated 2015-08-09 16:04:34

Parent: None

Type: Colorant

Weight: 304.0200
Formula Weight: 286.2070
LOI: 20.8800
Thermal Expansion: 0.0000
Oxide FeO Fe2O3
% Analysis 34.98 44.14
Formula 1.761 1.000

Crocus martis supplies Fe2O3.
A source of iron in glazes.
Analyses:
Hopper:
Fe2O3
Chappell:
Fe2O3 + impurities

Hazards

09/2016 Note: This is a new feature. If there is no safety information below, then that material's data has not yet been added. Some materials only have GHS ratings, while others only have HMIS ratings. Warnings differ between systems and countries. Glazy does not take any responsibility for accuracy of linked SDS information. Contact your ceramics supplier for safety information for your specific materials.

This material's safety information has not yet been added to Glazy.

Recipes using this material

Name Amount of Crocus martis Temp. Atmospheres Surface Transparency Si:Al R20:RO Author
Naomi Duffy Red 15 Δ6 14.36 0.2 : 0.8 Ceramic Recipes
Marno Green 3 Δ10 Reduction
Wood
Semi-glossy Opaque 8.99 0.35 : 0.65 Anglian Potters
Pot Camp Raku 7 Creamy Mustard 2 Δ06 Raku
Satin-matte Opaque 15.43 0.26 : 0.74 Anglian Potters
Pot Camp Raku 5 Mustard 4 Δ06 Raku
Satin Opaque 17.29 0.01 : 0.99 Anglian Potters
Red Orange 11.5 Δ6 Oxidation
Semi-matte Opaque 9.18 0.3 : 0.7 Terry Rorison
Penland Red Orange 11.5 Δ6 Semi-glossy 8.65 0.31 : 0.69 Glazy Admin
Mackersi Yellow 4.2 Δ6 Glossy 5.76 0.22 : 0.78 Glazy Admin