Created by Glazy Admin 2015-07-16 06:59:40, updated 2015-08-09 13:58:47

Parent: None

Type: Frit

Weight: 0.0000
Formula Weight: 262.4132
LOI: 0.0000
Thermal Expansion: 0.0000
Oxide SiO2 Al2O3 B2O3 CaO K2O Na2O
% Analysis 66.88 6.02 2.89 5.64 3.45 15.12
Formula 2.921 0.155 0.109 0.264 0.096 0.640

Frit 3110 supplies SiO2, Al2O3, B2O3, Na2O, CaO, and K2O.
Sodium borosilicate frit. High soda, low alumina.
Fusion at 1400F.
Similar frits: Pemco P-1505, Glostex GF-134, Fusion F-75.
Analyses:
Hopper:
% 2.5 K2O 15.4 Na2O 5.2 CaO 0.8 MgO 2.8 B2O3
3.7 Al2O3 69.6 SiO2
Cooper & Royle:
% 2.3 K2O 15.3 Na2O 6.3 CaO 2.6 B2O3 3.7 Al2O3 69.8 SiO2
Conrad:
0.064 K2O 0.643 Na2O 0.293 CaO 00981 B2O3
0.094 Al2O3 3.03 SiO2
Cushing:
0.06 K2O 0.65 Na2O 0.29 CaO 0.1 B2O3 0.1 Al2O3 3.0 SiO2
IMC:
% 2.3 K2O 15.3 Na2O 6.3 CaO 2.6 B2O3 3.7 Al2O3 69.8 SiO2
0.06 K2O 0.64 Na2O 0.29 CaO 0.10 B2O3 0.09 Al2O3 3.03 SiO2

Hazards

09/2016 Note: This is a new feature. If there is no safety information below, then that material's data has not yet been added. Some materials only have GHS ratings, while others only have HMIS ratings. Warnings differ between systems and countries. Glazy does not take any responsibility for accuracy of linked SDS information. Contact your ceramics supplier for safety information for your specific materials.

This material's safety information has not yet been added to Glazy.

Recipes using this material

Name Amount of Frit 3110 Temp. Atmospheres Surface Transparency Si:Al R20:RO Author
Val Cushing NDVC 6 Δ5 - 6 Reduction
Satin-matte 5.51 0.31 : 0.69 Glazy Admin
Lisa Orr's Base Cone--04 Glaze 66   Oxidation
14.8 0.75 : 0.25 Clemson University---Ceramic Dept.
Lisa Orr's Turquoise Cone--04 Glaze 66 Δ05 - 04 Oxidation
14.8 0.75 : 0.25 Clemson University---Ceramic Dept.
Lisa Orr's Molasses Cone--04 Glaze 66 Δ05 - 04 Oxidation
13.38 0.75 : 0.25 Clemson University---Ceramic Dept.
Lisa Orr's Honey Amber Cone--04 Glaze 66 Δ05 - 04 Oxidation
14.8 0.75 : 0.25 Clemson University---Ceramic Dept.
Basic Water Blue (Wright's) 59 Δ1 - 6 Oxidation
Glossy Translucent 12.7 0.63 : 0.37 Ginger Lukas
Steve's Clear Crackle (Plum) 40 Δ06 - 04 Wood
Semi-glossy Translucent 7.86 0.46 : 0.54 IU Southeast Ceramics
Steve's Clear Crackle 40 Δ06 - 04 Raku
Semi-glossy 7.86 0.46 : 0.54 IU Southeast Ceramics
black wax resist 25   18.85 0.74 : 0.26 Adam Yungbluth
Water Blue Revision 1 55 Δ6 Oxidation
Glossy Translucent 11.21 0.62 : 0.38 Ceramic Recipes
Water Blue Original 77 Δ6 Oxidation
Glossy Transparent 14.44 0.68 : 0.32 Ceramic Recipes
Bill's Best Light Green 54.2 Δ6 - 7 Oxidation
Glossy Semi-opaque 25.13 0.32 : 0.68 Triin Lehismets
Clear Base 2 Lisa Orr 73 Δ04 - 03 Oxidation
Glossy Transparent 9.63 0.63 : 0.37 Glazy Admin
Reactive glaze 58 Δ4 - 7 Oxidation
Reduction
Wood
Glossy Transparent 24.82 0.32 : 0.68 Clara Giorello
Rod's Sweetwater Warm 39.3 Δ5½ - 6 Oxidation
Semi-glossy Translucent 7.78 0.55 : 0.45 Rod Haaland
John's Goldstone 89 Δ5½ - 6 Oxidation
Glossy Transparent 17.88 0.82 : 0.18 Clara Giorello
Lok Ming Fung 75 Δ06 - 04 Oxidation
11.24 0.73 : 0.27 Matthew Mulholland
Heath Porcelain Casting Slip 2015 19 Δ6 4.21 0.69 : 0.31 Ceramic Recipes
Van Gilder's Tenmoku/Rana (variation without Crecer 804) 4.13 Δ6 - 7 Neutral
Glossy Opaque 9.08 0.23 : 0.77 Arline Edmonds
Van Gilder's Tenmoku/Rana (variation) 16.9 Δ6 - 7 Oxidation
Glossy Opaque 7.84 0.24 : 0.76 Stacey McDonald
Enchanted Forest 22.5 Δ5½ - 7 Oxidation
Neutral
Semi-glossy Semi-opaque 4.73 0.41 : 0.59 Tamas Ferencz
Tom Turner's copper Red 4.8 Δ9 - 10 Oxidation
Semi-glossy Semi-opaque 9.35 0.27 : 0.73 kenneth ibbett
Ferguson Copper Matte 13 Δ08 - 05½ Raku
Dry Matte 18.85 0.74 : 0.26 Jesse VanderBand
Rey Fa ^6 Crystaline Glaze 51   27.13 0.29 : 0.71 Ceramic Recipes
Opacified Steven Hill Clear with 1% Mason Stain 6388 (Mazerine) 4 Δ10 Reduction
Glossy Semi-opaque 8.8 0.25 : 0.75 IU Southeast Ceramics
Opacified Steven Hill Clear with 2% Mason Stain 6201 (Celadon) 4 Δ10 Reduction
Glossy Semi-opaque 8.8 0.25 : 0.75 IU Southeast Ceramics
Opacified Steven Hill Clear with 2% Mason Stain 6242 (Bermuda Green) 4 Δ10 Reduction
Glossy Semi-opaque 8.8 0.25 : 0.75 IU Southeast Ceramics
Opacified Steven Hill Clear with 3% Mason Stain 6108 (Walnut) 4 Δ10 Reduction
Glossy Semi-opaque 8.8 0.25 : 0.75 IU Southeast Ceramics
Opacified Steven Hill Clear (clear glaze with 7% Zircopax) 4 Δ10 Reduction
Glossy Translucent 8.8 0.25 : 0.75 IU Southeast Ceramics
John's Goldstone Zinc 58 Δ5½ Oxidation
Glossy Translucent 30.48 0.68 : 0.32 Clara Giorello
Snair Goldstone 61 Δ5½ Oxidation
Glossy Translucent 30.8 0.81 : 0.19 Clara Giorello
Rojo Marina SiC/3110 60 Δ5 Oxidation
Glossy Semi-opaque 5.03 0.73 : 0.27 Clara Giorello
John's Straw Ash 30.2 Δ6 Oxidation
Semi-glossy Opaque 17.16 0.36 : 0.64 Maciej Bednarczyk
Post's Jun White ^6 Glaze 17.4 Δ6 9.16 0.42 : 0.58 Ceramic Recipes
Steven Hill Clear 4 Δ10 Reduction
Glossy Transparent 8.47 0.25 : 0.75 IU Southeast Ceramics
VC Alkaline base 25 Δ6 Oxidation
Glossy 6.87 0.36 : 0.64 Alisa Liskin Clausen
VC Alkaline base, 1. 0 Copper carb 25 Δ6 Oxidation
Glossy 6.87 0.36 : 0.64 Alisa Liskin Clausen
VC Alkaline Mat, 5. 0 RIO ^5-6 25 Δ6 Oxidation
Glossy 6.87 0.36 : 0.64 Alisa Liskin Clausen
John's Straw Ash 30.2 Δ5 - 6 Oxidation
Semi-matte Opaque 17.16 0.36 : 0.64 Clara Giorello
MC6 High Expansion Glaze 19 Δ6 6.47 0.35 : 0.65 Ceramic Recipes