Created by Glazy Admin 2015-07-16 06:59:40, updated 2015-08-09 17:15:01

Parent: None

Type: Clay

Weight: 0.0000
Formula Weight: 0.0000
LOI: 4.8000
Thermal Expansion: 0.0000
Oxide SiO2 Al2O3 MgO CaO K2O Na2O P2O5 Fe2O3 TiO2
% Analysis 64.95 15.51 1.59 0.26 4.15 0.38 0.22 7.05 1.09
Formula 7.106 1.000 0.259 0.031 0.290 0.040 0.010 0.290 0.090

Red clay supplies SiO2, Al2O3, and Fe2O3.
Generic red clay. Map to a particular kind of red clay, or use
generic formula below.
Analyses: (generic Red Clay)
Green:
0.01 Na2O 0.10 K2O 0.07 MgO 0.08 CaO 1.0 Al2O3
3.52 SiO2 0.07 TiO2 0.22 Fe2O3 0.93 H2O

Hazards

09/2016 Note: This is a new feature. If there is no safety information below, then that material's data has not yet been added. Some materials only have GHS ratings, while others only have HMIS ratings. Warnings differ between systems and countries. Glazy does not take any responsibility for accuracy of linked SDS information. Contact your ceramics supplier for safety information for your specific materials.

This material's safety information has not yet been added to Glazy.

Recipes using this material

Name Amount of Red clay Temp. Atmospheres Surface Transparency Si:Al R20:RO Author
SA Orange Shino 10 Δ9 - 11 Reduction
Salt & Soda
Wood
Satin Opaque 4.65 0.95 : 0.05 Anglian Potters
Titanium Slip 10 Δ10 Wood
Matte Opaque 4.17 0.91 : 0.09 Anglian Potters
AC Lili Albany glaze ^6 ox. 2 Cobalt Carbonate plus 5 Rutile 20 Δ6 Oxidation
23.14 0.08 : 0.92 Alisa Liskin Clausen
AC Lili Albany glaze ^6 ox. 2 Cobalt Carbonate 20 Δ6 Oxidation
23.14 0.08 : 0.92 Alisa Liskin Clausen
AC Lili Albany glaze ^6 ox. no cobalt 20 Δ6 Oxidation
23.14 0.08 : 0.92 Alisa Liskin Clausen
AC Lili Albany glaze ^6 ox. no Cobalt, 5 Rutile 20 Δ6 Oxidation
Opaque 23.14 0.08 : 0.92 Alisa Liskin Clausen
AC Lili Red Art glaze, 2 co. ox. 20 Δ6 Oxidation
Opaque 23.14 0.08 : 0.92 Alisa Liskin Clausen
AC Lili Redart Glaze, 2 cobalt ox, 5 Rutile 20 Δ6 Oxidation
Opaque 23.14 0.08 : 0.92 Alisa Liskin Clausen
AC Lili Redart Glaze, 2 co. carb, 3 Rutile 20 Δ6 Oxidation
Semi-matte Opaque 23.14 0.08 : 0.92 Alisa Liskin Clausen
AC Albany slip glaze, 2 co. carb. 20 Δ6 Oxidation
Semi-glossy Opaque 14.58 0.2 : 0.8 Alisa Liskin Clausen
Delhi Blue Clay Body 2 10 Δ9 - 11 2.88 0.51 : 0.49 Ceramic Recipes
Red Art Mix 84.16   Oxidation
Semi-glossy Semi-opaque 7.11 0.17 : 0.83 Alisa Liskin Clausen
Vero 354 Shino 40 Δ5 Oxidation
Semi-glossy Translucent 9 0.49 : 0.51 Clara Giorello
Gold Metallic 86 Δ5 - 6 Oxidation
Semi-matte Opaque 7.53 0.53 : 0.47 Clara Giorello
Manganese Bronze 60   Oxidation
Satin Opaque 9.79 0.37 : 0.63 Clara Giorello
C/Azul - NG 24.04 Δ5 - 9 Oxidation
Wood
Satin-matte Opaque 8.75 0.25 : 0.75 Clara Giorello
Malcom Davis Shino 5.8 Δ5 - 6 Reduction
3.84 0.96 : 0.04 Clara Giorello
Speckled White-Green Glaze 5 Δ9 - 10 Oxidation
Reduction
Matte Opaque 4.26 0.26 : 0.74 Derek Au
Bronze Metallic 55 Δ04 - 03 Oxidation
Matte Opaque 7.58 0.53 : 0.47 Glazy Admin
Amber New Tyler 60 Δ6 Oxidation
Glossy 8.76 0.43 : 0.57 Glazy Admin
Shino June Perry's #789 Orange 2.44 Δ9 Reduction
5 0.95 : 0.05 Glazy Admin
IE 68 13.48 Δ6 Oxidation
Semi-matte 5.57 0.28 : 0.72 Glazy Admin
Bronze Ogden 66.67 Δ6 Oxidation
Matte Opaque 4.22 0.53 : 0.47 Glazy Admin
Synthetic Esturine Mud 23.39 Δ8 - 10 Oxidation
Reduction
6.99 0.17 : 0.83 Glazy Admin
Green Veerkamp 1 21.7 Δ10 Reduction
Glossy Translucent 7.35 0.22 : 0.78 Glazy Admin
Gold Metallic 86.7 Δ6 Oxidation
Matte Opaque 7.51 0.53 : 0.47 Glazy Admin
Nikom Altered 1 7.03 Δ2 - 6 Oxidation
Reduction
Glossy 20.21 0.42 : 0.58 Glazy Admin
Gluskoter's Dry Ash Glaze 30 Δ10 Reduction
3.56 0.4 : 0.6 Glazy Admin
Peach Bloom Glaze 1.96 Δ9 Oxidation
Reduction
13.84 0.23 : 0.77 Glazy Admin
AG 19 50 Δ6 Reduction
8.49 0.4 : 0.6 Glazy Admin
Nikom 16.67 Δ2 - 6 Oxidation
Reduction
Glossy 24.83 0.42 : 0.58 Glazy Admin
Olive Matte 11 Δ5 - 8 Oxidation
Reduction
Matte 6.76 0.14 : 0.86 Glazy Admin