Created by Glazy Admin 2015-07-16 06:59:40, updated 2015-08-09 17:22:07

Parent: None

Type: Colorant

Weight: 88.8660
Formula Weight: 88.6489
LOI: 0.1000
Thermal Expansion: 14.2100
Oxide Fe2O3 TiO2
% Analysis 9.90 90.00
Formula 0.055 1.000

Rutile supplies TiO2 and Fe2O3.
Natural source of titanium with iron impurities. (Parmelee
indicates that up to 25% FeO may be in solution in the crystal.)
Rutile may also contain silica, chromium, and vanadium. Can be
very fluid in reduction [Memmott].
Analyses:
Hopper:
TiO2
Chappell: (questionable)
FeTiO3
Memmott:
TiO2 with iron traces
IMC: (no iron?)
% 96.10 TiO2 0.90 ZrO2 0.30 Al2O3 0.10 LOI

Hazards

09/2016 Note: This is a new feature. If there is no safety information below, then that material's data has not yet been added. Some materials only have GHS ratings, while others only have HMIS ratings. Warnings differ between systems and countries. Glazy does not take any responsibility for accuracy of linked SDS information. Contact your ceramics supplier for safety information for your specific materials.
Globally Harmonized System (GHS) Hazardous Materials Identification System (HMIS) SDS Link
Pictograms Signal Word Hazard Statements Health Flammability Hazard Protection
1 0 0

Recipes using this material

Name Amount of Rutile Temp. Atmospheres Surface Transparency Si:Al R20:RO Author
rutile ash 15 Δ5 - 10 Oxidation
Reduction
Salt & Soda
Semi-matte 27.36 0.3 : 0.7 timothy graham
Early Spring Green 2 Δ5½ - 7 Neutral
Glossy Translucent 9.31 0.2 : 0.8 Arline Edmonds
Devon frozen water 2 Δ5½ - 7 Oxidation
Semi-matte Semi-opaque 10.57 0.19 : 0.81 Tom Demeranville
Woo Blue Brown 4 Δ10 Reduction
Glossy 9.38 0.29 : 0.71 Glazy Admin
Pumpkin 3.88 Δ10 Reduction
4.66 0.23 : 0.77 Glazy Admin
Sue's Blue -new (Cedar Hill) 5 Δ6 Oxidation
Matte Opaque 5.38 0.19 : 0.81 Sue McLeod
Blue -old (Cedar Hill) 400 Δ6 Oxidation
Matte Opaque 7.32 0.14 : 0.86 Sue McLeod
Sue's Green -new (Cedar Hill) 5 Δ6 Oxidation
Matte Opaque 5.17 0.15 : 0.85 Sue McLeod
Green -old (Cedar Hill) 5 Δ6 Oxidation
Matte Opaque 7.32 0.14 : 0.86 Sue McLeod
Sapphire Blue (Cedar Hill) 4 Δ6 Oxidation
Glossy Opaque 7.82 0.42 : 0.58 Sue McLeod
Raw Sienna (Cedar Hill) 6 Δ6 Oxidation
Reduction
Glossy 6.94 0.1 : 0.9 Sue McLeod
Floating Blue 4 Δ5 - 6 Oxidation
Semi-glossy Semi-opaque 7.01 0.47 : 0.53 mitch henke
Chance's Opal 7 Δ10 Oxidation
Reduction
Glossy Translucent 8.05 0.14 : 0.86 chance taylor
Sunny Yellow 6 Δ5½ - 6 Oxidation
Satin Opaque 4.55 0.35 : 0.65 Lisa Cotterman
WWW 237 M1 (variation) 5 Δ5 - 6 Oxidation
Neutral
Glossy Opaque 6.11 0.26 : 0.74 mitch henke
Fish Guts 0.5 Δ9 - 10 Reduction
Glossy Opaque 9.96 0.22 : 0.78 Sid Henderson
Shaner's Honey 3 Δ9 - 10 Reduction
Matte Opaque 6 0.34 : 0.66 Sid Henderson
Chappell Floating Blue, Blue Hare (variation) 4 Δ5 - 6 Oxidation
Glossy 7.01 0.48 : 0.52 mitch henke
Sun Valley 7.01 Δ9 - 12 Reduction
Glossy Opaque 7.7 0.22 : 0.78 Mark Quinto
Variegated Slate Blue 6 Δ6 Oxidation
Glossy Translucent 6.39 0.09 : 0.91 Joe Thompson
MSU Copper Red 0.1 Δ9 Reduction
Glossy Opaque 10.58 0.33 : 0.67 Morehead State University
Glossy Yellow with Blue Crystals 4.01 Δ6 Oxidation
Semi-glossy 15.28 0.32 : 0.68 Ginger Lukas
Leach 4321 variation (+2 RIO, 2 Lt Rutile, 2 ZincOX, 2 Volclay, 5 OM4) 2 Δ8 - 10 Reduction
Glossy Semi-opaque 9.06 0.22 : 0.78 Rodney Johnson
Hobbs Peachbloom #1 2 Δ6 - 8 Reduction
Semi-glossy Semi-opaque 11.05 0.33 : 0.67 Ryan Hobbs
Hobbs Turquiose 2 Δ6 Oxidation
Glossy Translucent 10.85 0.33 : 0.67 Ryan Hobbs
Spearmint Green 6 Δ6 Oxidation
Neutral
Glossy Translucent 7.96 0.13 : 0.87 Joe Thompson
Apple Cinnamon 3.09 Δ5 - 6 Oxidation
Glossy Opaque 7.88 0.52 : 0.48 Stacey McDonald
Persimmon Celadon 3 Δ6 Oxidation
Semi-glossy Translucent 8.64 0.43 : 0.57 Ginger Lukas
Icing Pink 3.5 Δ6 Oxidation
Semi-matte 17.32 0.51 : 0.49 Glazy Admin
R4 Azul Rut 5 Δ4 - 5 Oxidation
Glossy Opaque 6.45 0.19 : 0.81 Clara Giorello
Honey Clear 6 Δ6 8.48 0.28 : 0.72 Glazy Admin
Transparent Semi-matte 1.7 Δ5 - 6 Oxidation
Reduction
10.79 0.13 : 0.87 Glazy Admin
Lalone Blue Ash (toms gb variation) 0.5 Δ5 - 6 Oxidation
Satin-matte Semi-opaque 6.82 0.28 : 0.72 Tom Demeranville
SWIC Eggshell 7 Δ6 Oxidation
Semi-matte Opaque 5.5 0.22 : 0.78 Jake Bish
WWW 237 M1 (variation) 5 Δ6 Oxidation
Neutral
Glossy Opaque 5.93 0.26 : 0.74 Triin Lehismets
Westcountry apple sauce 6 Δ5½ - 7 Oxidation
Semi-glossy Translucent 7.82 0.69 : 0.31 Tom Demeranville
Lynette's Opal 8 Δ5 - 7 Oxidation
Glossy Semi-opaque 7.86 0.28 : 0.72 Triin Lehismets
Jurassic Green 6 Δ6 Oxidation
Semi-matte Semi-opaque 6.66 0.13 : 0.87 Dan Lizotte
Cretaceous Blue 5 Δ6 Oxidation
Semi-matte Semi-opaque 6.66 0.13 : 0.87 Dan Lizotte
Reitz Chamelion 2 Δ10 - 11 Oxidation
Reduction
Smooth Matte Opaque 4.83 0.71 : 0.29 Sid Henderson