Created by Glazy Admin 2016-02-14 11:27:09, updated 2016-02-14 11:27:09

Weight: 0.0000
Formula Weight: 460.1141
LOI: 2.0000
Thermal Expansion: 0.0000
Oxide SiO2 Al2O3 K2O Na2O Fe2O3
% Analysis 58.47 23.19 8.57 7.56 0.20
Formula 4.569 1.068 0.427 0.573 0.006

Information from Digitalfire:

https://digitalfire.com/4sight/material/nepheline_syenite_norwegian_2940.html

Hazards

09/2016 Note: This is a new feature. If there is no safety information below, then that material's data has not yet been added. Some materials only have GHS ratings, while others only have HMIS ratings. Warnings differ between systems and countries. Glazy does not take any responsibility for accuracy of linked SDS information. Contact your ceramics supplier for safety information for your specific materials.

This material's safety information has not yet been added to Glazy.

Recipes using this material

Name Amount of Nepheline Syenite Norwegian Temp. Atmospheres Surface Transparency Si:Al R20:RO Author
Toms turquoise matte 26.5 Δ6 - 7 Oxidation
Satin-matte Opaque 4.9 0.33 : 0.67 Tom Demeranville
Toms crack bubble white 44.5 Δ6 - 8 Oxidation
Semi-glossy Opaque 5.3 0.67 : 0.33 Tom Demeranville
Lynette's Opal 38 Δ5 - 7 Oxidation
Glossy Semi-opaque 7.86 0.28 : 0.72 Triin Lehismets
Kitten's Clear Blue 24 Δ6 Oxidation
Glossy Translucent 10.51 0.22 : 0.78 Triin Lehismets
Burnt Marshmallow 50.8 Δ10 Oxidation
Stony Matte Opaque 3.71 0.26 : 0.74 Matt Katz
NR 39 73 Δ6 - 11 Oxidation
Reduction
Wood
Semi-glossy Translucent 4.98 0.57 : 0.43 Triin Lehismets
Triin's Tenmoku Gold 14.4 Δ6 - 7 Oxidation
Glossy Translucent 10.48 0.39 : 0.61 Triin Lehismets
SA Orange Shino 33 Δ9 - 11 Reduction
Salt & Soda
Wood
Satin Opaque 4.65 0.95 : 0.05 Anglian Potters
Triin's Icing Pink 25.7 Δ6 - 7 Oxidation
Semi-glossy Opaque 16.95 0.35 : 0.65 Triin Lehismets
Triin's Cherry Blossom Pink 26.2 Δ6 Oxidation
Satin Opaque 16.16 0.36 : 0.64 Triin Lehismets
Mo's White Shino 75 Δ10 Wood
Semi-glossy Semi-opaque 4.6 0.61 : 0.39 Anglian Potters
Shino D 70 Δ9 - 10 Oxidation
Reduction
Wood
Glossy Translucent 4.7 0.98 : 0.02 Ruth Gillett
Shino C Pot Camp standard 35 Δ9 - 10 Oxidation
Reduction
Wood
Glossy Translucent 4.26 0.97 : 0.03 Ruth Gillett
Shino A shiny 35 Δ9 - 10 Oxidation
Reduction
Wood
Glossy Semi-opaque 4.19 0.98 : 0.02 Ruth Gillett
HVAR Shino #3 1 Δ10 - 12 Salt & Soda
Wood
Satin Semi-opaque 4.58 Anglian Potters
Strontium Blue 56 Δ6 - 8 Oxidation
Satin-matte Semi-opaque 5.13 0.53 : 0.47 Triin Lehismets
Kittens Clear base 24 Δ6 Oxidation
Glossy Transparent 10.95 0.23 : 0.77 Alicia Cook
Crackle White 20 Δ07 - 06 Raku
Satin Opaque 4.56 0.11 : 0.89 Anglian Potters
Dark Shino #5 33.3 Δ10 - 12 Salt & Soda
Wood
Semi-glossy Semi-opaque 4.65 0.97 : 0.03 Anglian Potters
crystaline base 21.74 Δ9 Oxidation
Glossy Transparent 11.25 0.33 : 0.67 Ruth Gillett
Triin's speckled rutile yellow 15.5 Δ6 - 8 Oxidation
Glossy Semi-opaque 9.06 0.24 : 0.76 Triin Lehismets
Triin's rutile yellow 15.5 Δ6 - 8 Oxidation
Glossy Semi-opaque 9.06 0.24 : 0.76 Triin Lehismets
John's cash blue rev 32.8 Δ6 - 8 Oxidation
Semi-glossy Semi-opaque 13.09 0.39 : 0.61 Triin Lehismets
Kitten's Clear green 24 Δ6 Oxidation
Glossy Translucent 10.51 0.22 : 0.78 Triin Lehismets
Kitten's Clear blue/green 24 Δ6 Oxidation
Glossy Translucent 10.51 0.22 : 0.78 Triin Lehismets
Kitten's Clear nutmeg 24 Δ6 Oxidation
Glossy Opaque 10.51 0.22 : 0.78 Triin Lehismets
Kitten's Clear light blue 24 Δ6 Oxidation
Glossy Transparent 10.51 0.22 : 0.78 Triin Lehismets
Kitten's Clear floating blue 24 Δ6 Oxidation
Glossy Translucent 10.51 0.22 : 0.78 Triin Lehismets
Kitten's Clear rutile blue 24 Δ6 Oxidation
Glossy Translucent 10.51 0.22 : 0.78 Triin Lehismets
Soda tan mauve 24 Δ9 Oxidation
Glossy Transparent 9.03 0.36 : 0.64 Ruth Gillett
Kittens Clear Base w/Sage Green 24 Δ6 Oxidation
Glossy Transparent 10.95 0.23 : 0.77 Alicia Cook