Category: Glaze > Iron > Celadon > Blue
Created 2018-01-10 04:51:16 by Hailey Smither
Categories: Glaze > Iron > Celadon > Blue
Firing Temperature: Δ9-10
Atmospheres: Reduction
Surface Type: Glossy
Transparency: Translucent

Material Amount Batch Subtotal
Custer Feldspar 52
Whiting 21
Silica 20
Amtalc-C98 Talc 3
Tricalcium Phosphate, Synthetic Bone Ash 2
Total Base:98
Yellow Ochre 2
Total: 100

Percentage Analysis

Ingredient Amount SiO2 Al2O3 MgO CaO K2O Na2O KNaO P2O5 Fe2O3 TiO2 LOI
Custer Feldspar5235.628.840.165.21.566.760.050.16
Whiting2111.789.22
Silica2020
Amtalc-C98 Talc31.610.010.890.110.010.010.020.36
Tricalcium Phosphate, Synthetic Bone Ash21.080.92
Yellow Ochre21.160.40.44
Total10058.389.250.8913.135.211.566.770.920.5109.74
100% no LOI 64.9810.290.9914.625.81.747.531.020.560

Unity Molecular Formula (UMF)

FLUXES

RO/R2O

0.08 Na2O
0.17 K2O
0.69 CaO
0.07 MgO
STABILIZERS

R2O3

0.27 Al2O3
GLASS-FORMERS

RO2

2.89 SiO2
OTHER

 

0.01 Fe2O3
0.02 P2O5
SILICA:ALUMINA

SiO2:Al2O3

10.68

FLUX RATIO

R2O:RO

0.24 : 0.76

SiO2:Al2O3 Chart

Closest 40 neighbors in Glaze > Iron > Celadon > Blue.

Click and drag to zoom
Stull Chart
SiO2:Al2O3 Ratio
SiO2:Al2O3 Ratio 10.68

Similar Base Recipes

No recipes with similar base ingredients and amounts were found.

Similar RO/R2O Unity Formulas

R2O3 - STABILIZERS RO2 - GLASS FORMERS RO/R2O - FLUXES
Recipe Name ΔTemp Al2O3 B2O3 SiO2 ZrO2 SnO2 TiO2 KNaO K2O Na2O CaO MgO ZnO BaO PbO Li2O SrO
Korean Blue Celadon 9-10 0.27 2.89 0.25 0.17 0.08 0.69 0.07
Phil Roger's Synthetic Nuka 10 0.23 0.03 2.92 0.21 0.19 0.02 0.74 0.05

No reviews yet.

Hazards

09/2016 Note: This is a new feature. If a recipe material is not listed, that material's data has not yet been added. Some materials only have GHS ratings, while others only have HMIS ratings. Warnings differ between systems and countries. Glazy does not take any responsibility for accuracy of linked SDS information. Contact your ceramics supplier for safety information for your specific materials.
Globally Harmonized System (GHS) Hazardous Materials Identification System (HMIS) SDS Link
Material Pictograms Signal Word Hazard Statements Health Flammability Hazard Protection
Custer Feldspar HarmfulHealth Hazard WARNING May cause damage to lungs through prolonged or repeated inhalation.
Suspected of causing cancer through
prolonged or repeated inhalation.
May cause allergy or asthma symptoms or breathing difficulties if inhaled.
May cause skin or eye irritation.
Whiting Harmful WARNING Causes eye irritation
Silica HarmfulHealth Hazard DANGER From 200-Mesh SDS:
May cause cancer by inhalation.
Causes damage to lungs through prolonged or repeated exposure by inhalation.
* 0 0 E
Amtalc-C98 Talc Harmful WARNING Causes mild skin irritation
Harmful if inhaled
May cause respiratory irritation
1 0 0 E
Tricalcium Phosphate, Synthetic Bone Ash 1 0 0 D
Yellow Ochre Health Hazard DANGER May cause cancer.