Category: Glaze > Shino > White
Created 2016-11-19 19:36:04 by Anglian Potters
Categories: Glaze > Shino > White
Firing Temperature: Δ10
Atmospheres: Wood
Surface Type: Glossy - Semi
Transparency: Semi-opaque

Used by Anglian Potters at their annual camp, fired on members pots in the wood kiln. in 2017 we found that applied thickly to bodies containing at least some Special fleck this gave an attractive double layer crazing

Material Amount Batch Subtotal
Nepheline Syenite Norwegian 75
Talc (Theoretical) 15
Kaolin (Theoretical) 10
Total Base:100
Salt 3
Total: 103

Percentage Analysis

Ingredient Amount SiO2 Al2O3 MgO K2O Na2O KNaO Fe2O3 LOI
Nepheline Syenite Norwegian7543.8517.46.435.6712.10.151.5
Talc (Theoretical)159.514.780.71
Kaolin (Theoretical)104.734.021.25
Salt31.591.591.41
Total10358.0921.424.786.437.2613.690.154.87
100% no LOI 59.221.824.876.557.413.950.16

Unity Molecular Formula (UMF)

FLUXES

RO/R2O

0.39 Na2O
0.22 K2O
0.39 MgO
STABILIZERS

R2O3

0.69 Al2O3
GLASS-FORMERS

RO2

3.18 SiO2
SILICA:ALUMINA

SiO2:Al2O3

4.60

FLUX RATIO

R2O:RO

0.61 : 0.39

SiO2:Al2O3 Chart

Closest 2 neighbors in Glaze > Shino > White.

Click and drag to zoom
Stull Chart
SiO2:Al2O3 Ratio
SiO2:Al2O3 Ratio 4.6

Similar Base Recipes

No recipes with similar base ingredients and amounts were found.

Similar RO/R2O Unity Formulas

No recipes with similar RO/R2O Unity Formulas were found.

No reviews yet.

Hazards

09/2016 Note: This is a new feature. If a recipe material is not listed, that material's data has not yet been added. Some materials only have GHS ratings, while others only have HMIS ratings. Warnings differ between systems and countries. Glazy does not take any responsibility for accuracy of linked SDS information. Contact your ceramics supplier for safety information for your specific materials.
Globally Harmonized System (GHS) Hazardous Materials Identification System (HMIS) SDS Link
Material Pictograms Signal Word Hazard Statements Health Flammability Hazard Protection
Talc (Theoretical) Harmful WARNING Causes mild skin irritation
Harmful if inhaled
May cause respiratory irritation
1 0 0 E
Kaolin (Theoretical) HarmfulHealth Hazard DANGER SDS for EPK KAOLIN: EPK Kaolin is a naturally occurring mineral, which may contain amounts of crystalline silica
typically 0.1-1.0%, may cause damage to respiratory system through prolonged or repeated
exposure.