Category: Glaze > Shino
Created 2017-05-16 01:45:53 by Lee Love
Categories: Glaze > Shino
Firing Temperature: Δ9-11
Atmospheres: Reduction
Surface Type: Glossy - Semi
Transparency: Semi-opaque

Cone 9 and up. Reduction before cone 012.

NephSy 50
Spodumene 26
EPK 6
OM4 8.4
Kona F4 6.2
Soda Ash 4

Material Amount Batch Subtotal
Nepheline Syenite (Theoretical) 50
Spodumene (Theoretical) 26
Kentucky OM #4 Ball Clay 8.4
Kona F-4 feldspar 6.2
EPK 6
Soda Ash 4
Total Base:100.6
Red iron oxide 3
Total: 103.6

Percentage Analysis

Ingredient Amount SiO2 Al2O3 MgO CaO Li2O K2O Na2O KNaO P2O5 Fe2O3 TiO2 LOI
Nepheline Syenite (Theoretical)5030.3511.650.050.352.34.97.20.050.35
Spodumene (Theoretical)2616.797.132.08
Kentucky OM #4 Ball Clay8.44.642.340.030.030.080.030.110.090.11.06
Kona F-4 feldspar6.24.141.210.110.30.430.730.01
EPK62.742.240.010.010.020.020.020.050.020.89
Soda Ash4222
Red iron oxide32.850.15
Total103.658.6624.570.090.492.082.77.3610.060.023.040.124.46
100% no LOI 59.1724.790.090.52.12.737.4210.150.023.070.12

Unity Molecular Formula (UMF)

FLUXES

RO/R2O

0.52 Na2O
0.13 K2O
0.31 Li2O
0.04 CaO
0.01 MgO
STABILIZERS

R2O3

1.06 Al2O3
GLASS-FORMERS

RO2

4.28 SiO2
0.01 TiO2
OTHER

 

0.08 Fe2O3
SILICA:ALUMINA

SiO2:Al2O3

4.05

FLUX RATIO

R2O:RO

0.95 : 0.05

SiO2:Al2O3 Chart

Closest 100 neighbors in Glaze > Shino.

Click and drag to zoom
Stull Chart
SiO2:Al2O3 Ratio
SiO2:Al2O3 Ratio 4.05

Similar Base Recipes

No recipes with similar base ingredients and amounts were found.

Similar RO/R2O Unity Formulas

R2O3 - STABILIZERS RO2 - GLASS FORMERS RO/R2O - FLUXES
Recipe Name ΔTemp Al2O3 B2O3 SiO2 ZrO2 SnO2 TiO2 KNaO K2O Na2O CaO MgO ZnO BaO PbO Li2O SrO
NCC Shop Shino + 3% Red Iron Oxide 9-11 1.06 4.28 0.01 0.65 0.13 0.52 0.04 0.01 0.31
Shino Linda's 9-10 1.04 4.26 0.01 0.66 0.11 0.55 0.03 0.01 0.3
Linda's Pink Shino 10 1.04 4.26 0.01 0.66 0.11 0.55 0.03 0.01 0.3

No reviews yet.

Hazards

09/2016 Note: This is a new feature. If a recipe material is not listed, that material's data has not yet been added. Some materials only have GHS ratings, while others only have HMIS ratings. Warnings differ between systems and countries. Glazy does not take any responsibility for accuracy of linked SDS information. Contact your ceramics supplier for safety information for your specific materials.
Globally Harmonized System (GHS) Hazardous Materials Identification System (HMIS) SDS Link
Material Pictograms Signal Word Hazard Statements Health Flammability Hazard Protection
Spodumene (Theoretical) Health Hazard DANGER May cause cancer by inhalation.
Causes damage to organs through prolonged or repeated exposure.
Kentucky OM #4 Ball Clay Health Hazard WARNING May cause damage to lung through prolonged or repeated inhalation 2 0 0 E
EPK HarmfulHealth Hazard DANGER EPK Kaolin is a naturally occurring mineral, which may contain amounts of crystalline silica
typically 0.1-1.0%, may cause damage to respiratory system through prolonged or repeated
exposure.
1 0 0 E
Soda Ash Harmful WARNING Causes skin irritation.
Causes serious eye irritation.
2 0 0 B
Red iron oxide Health Hazard WARNING May cause damage to lung through prolonged or repeated exposure by inhalation