Glaze, 4706 recipes

Name Temp. Atmospheres Surface Transparency Si:Al R20:RO Author Rating
DEV 001a M2 Δ6 Oxidation
Glossy Opaque 13.05 0.39 : 0.61 Daniel Spruyt
Heino Turquoise ^10 (variation) Δ10 Satin-matte Opaque 4.95 0.53 : 0.47 Glazy Admin
Pinker Paler Δ8 - 11 Oxidation
Glossy Transparent 10.2 0.14 : 0.86 david tsabar
Dirty Snow ^6 Glaze Δ6 8.39 0.21 : 0.79 Ceramic Recipes
Selsor Chun SiC, RIO 0.5/1/1.5/2 Δ5 Oxidation
Glossy Semi-opaque 15.12 0.26 : 0.74 Clara Giorello
Selsor Chun, RIO 0.5/1/1.5/2 Δ5 Reduction
15.12 0.26 : 0.74 Clara Giorello
Van Gilder's Tenmoku/Rana (variation without Crecer 804) Δ6 - 7 Neutral
Glossy Opaque 9.08 0.23 : 0.77 Arline Edmonds
Nutmeg Shino Cone 6 Sugar Maples (Toms UK GB variation) Δ6 Oxidation
Satin Opaque 7.06 0.21 : 0.79 Tom Demeranville
Dirty snow (Toms GB/Strontium Variation) Δ6 - 7 Oxidation
8.6 0.19 : 0.81 Tom Demeranville
Selsor Waxy White Liner (Toms variation) Δ6 Oxidation
Reduction
Semi-glossy 7.37 0.2 : 0.8 Tom Demeranville
Pete Pinnell Clear Adjusted with Cobalt Δ10 - 11 Oxidation
Reduction
Glossy Translucent 8.64 0.2 : 0.8 Derek Au
Pete Pinnell Clear Adjusted with Cobalt (sub MgO for CaO) Δ10 - 11 Oxidation
Reduction
Satin Semi-opaque 8.62 0.2 : 0.8 Derek Au
P7.P9.D2/3 Temmoku Δ8 Reduction
Glossy Opaque 7.67 0.25 : 0.75 Andrea Campioni
P50.B2.Ca Δ8 Reduction
Semi-glossy Semi-opaque 10.32 0.12 : 0.88 Andrea Campioni
P41P42.B2.Ca. Elba island Celadon Δ8 Reduction
Glossy Translucent 9.54 0.02 : 0.98 Andrea Campioni
200.3.15 Mg Δ8 Reduction
Glossy Transparent 8.48 0.21 : 0.79 Andrea Campioni
P47.P19.B2 red temmoku Δ8 Reduction
Smooth Matte Opaque 9.48 0.38 : 0.62 Andrea Campioni
Waxy white Shino Δ7 - 8 Oxidation
Satin-matte Translucent 4.14 0.96 : 0.04 Made in Mokum
Pumice celadon (Barium) Δ9 - 11 Reduction
Glossy Translucent 9.8 0.19 : 0.81 david tsabar
Rich's Turquoise Δ08 - 05½ Raku
Glossy Opaque 5.96 0.7 : 0.3 Jesse VanderBand
Soldner Red Raku Δ08 - 05½ Raku
25.06 0.43 : 0.57 Jesse VanderBand
Alligator Raku Δ05½ - 04 Raku
Opaque 25.06 0.09 : 0.91 Glazy Admin
Cone 6 Pink (variation) Δ5 - 7 Oxidation
Glossy Translucent 10.58 0.16 : 0.84 Stacey McDonald
Triin's rutile yellow (variation: sub Hyplas 71 ball clay with OM 4) Δ6 - 8 Oxidation
Glossy Semi-opaque 9.06 0.24 : 0.76 Arline Edmonds
Ocean Trench Blue Δ5 - 6 Oxidation
Satin-matte Opaque 6.75 0.09 : 0.91 Jesse VanderBand
Aquatic Blue Δ9 - 10 Reduction
Matte Opaque 5.4 0.33 : 0.67 Jason Burke
Kitten's Clear blue/green (Bunty's variation) Δ6 Oxidation
Glossy Translucent 10.78 0.21 : 0.79 Jayne Bunting
Bunty's British Variation of Kitten's Clear Green Δ5 - 6 Oxidation
Glossy Translucent 10.53 0.31 : 0.69 Jayne Bunting
Burke's Strong Celadon Δ6 Oxidation
Glossy Transparent 8.38 0.28 : 0.72 Amber York
Van Gilder's Tenmoku/Rana (variation) Δ6 - 7 Oxidation
Glossy Opaque 7.84 0.24 : 0.76 Stacey McDonald
Rutile Green Δ6 Oxidation
Glossy Semi-opaque 10.55 0.31 : 0.69 Stacey McDonald
Cream Rust Δ6 Oxidation
Glossy Opaque 13.58 0.28 : 0.72 Stacey McDonald
Xavier Revised: CuOx 3.5 Rutile 4.5 Δ5 - 6 Oxidation
8.45 0.2 : 0.8 Clara Giorello
Akiko's crater glaze Δ6 - 8 Oxidation
Matte Opaque 4.76 0.55 : 0.45 kenneth ibbett
Bunty's British Variation of Kitten's Clear Bermuda Δ5 - 6 Oxidation
Glossy Translucent 10.78 0.21 : 0.79 Jayne Bunting
Bunty's Variation of Kitten's Clear Blue Rutile Δ5 - 6 Oxidation
Glossy Translucent 10.78 0.21 : 0.79 Jayne Bunting
Bunty's British Variation of Kitten's Clear Δ5 - 6 Oxidation
Glossy 10.78 0.21 : 0.79 Jayne Bunting
Enchanted Forest Δ5½ - 7 Oxidation
Neutral
Semi-glossy Semi-opaque 4.73 0.41 : 0.59 Tamas Ferencz
TFF Clear Δ5 - 6 Oxidation
Neutral
Glossy Transparent 8.43 0.25 : 0.75 Tamas Ferencz
NCC Shop Shino + 3% Red Iron Oxide Δ9 - 11 Reduction
Semi-glossy Semi-opaque 4.05 0.95 : 0.05 Lee Love