Glazy Admin, 3549 recipes

Name Temp. Atmospheres Surface Transparency Si:Al R20:RO Author Rating
Val Cushing NDVC Δ5 - 6 Reduction
Satin-matte 5.51 0.31 : 0.69 Glazy Admin
Clear Buttery Grandey Δ6 Oxidation
Satin Transparent 5.55 0.24 : 0.76 Glazy Admin
Edwards Waxy Clear Δ6 Glossy 14.35 0.21 : 0.79 Glazy Admin
Roy Clear 1 Δ6 Semi-glossy 7.97 0.16 : 0.84 Glazy Admin
Woo Blue Brown Δ10 Reduction
Glossy 9.38 0.29 : 0.71 Glazy Admin
Pumpkin Δ10 Reduction
4.66 0.23 : 0.77 Glazy Admin
Purple Haze Δ10 Reduction
Satin Opaque 10.14 0.25 : 0.75 Glazy Admin
Clear bob's base Δ7 - 8 Oxidation
Reduction
Glossy Transparent 8.2 0.13 : 0.87 Glazy Admin
Val Cushing V.C. Celadon Lung Chuan Δ9 - 10 Reduction
Semi-glossy Translucent 10.84 0.23 : 0.77 Glazy Admin
Strontium Blue Δ6 Matte 4.8 0.45 : 0.55 Glazy Admin
Pink Nickel Δ6 Oxidation
Matte Opaque 8.59 0.21 : 0.79 Glazy Admin
Hamer Bristol Δ6 Oxidation
Semi-matte Semi-opaque 5.39 0.37 : 0.63 Glazy Admin
Lewing Raspberry Δ6 Oxidation
Glossy 10.77 0.16 : 0.84 Glazy Admin
Chrome Tin Base Raspberry Blue Δ6 Glossy 8.31 0.19 : 0.81 Glazy Admin
Behrens Barium Base Δ6 Oxidation
Glossy 9.83 0.19 : 0.81 Glazy Admin
Icing Pink Δ6 Oxidation
Semi-matte 17.32 0.51 : 0.49 Glazy Admin
NCECA Clear Base Soft Blue Δ6 Glossy 8.74 0.24 : 0.76 Glazy Admin
Galloway Some Bright Base Δ6 Oxidation
Matte 6 0.14 : 0.86 Glazy Admin
Honey Clear Δ6 8.48 0.28 : 0.72 Glazy Admin
Val Cushing V.C. Matte Awsome KK Revised Δ6 Oxidation
Matte 4.95 0.17 : 0.83 Glazy Admin
Pink Bright Δ6 - 7 Oxidation
Satin-matte Opaque 5.71 0.55 : 0.45 Glazy Admin
Crystalline Black Δ6 Matte 7.19 0.1 : 0.9 Glazy Admin
BUTTERSCOTCH GLOSSY Δ6 Oxidation
Glossy 9.7 0.43 : 0.57 Glazy Admin
Black crystal no gb Δ5 - 6 Oxidation
Satin-matte Opaque 5.67 0.24 : 0.76 Glazy Admin
Transparent Semi-matte Δ5 - 6 Oxidation
Reduction
10.79 0.13 : 0.87 Glazy Admin
Matte B from Geoff Wheeler Δ6 Oxidation
Satin-matte Translucent 5.09 0.45 : 0.55 Glazy Admin
Gloss Base Bill Aycock's no GB Δ6 Oxidation
Reduction
Glossy Translucent 13.91 0.31 : 0.69 Glazy Admin
Clear Base 2 Lisa Orr Δ04 - 03 Oxidation
Glossy Transparent 9.63 0.63 : 0.37 Glazy Admin
Moonlight Δ10 Reduction
Glossy 8.1 0.28 : 0.72 Glazy Admin
Green Beth's Shiny Δ5 - 7 Oxidation
7.86 0.38 : 0.62 Glazy Admin
Val Cushing V.C. Matte 3 Δ5 - 6 Oxidation
Reduction
Satin-matte Translucent 5.8 0.21 : 0.79 Glazy Admin
Dolita Clear Base Δ6 5.56 0.31 : 0.69 Glazy Admin
Orange Red Δ6 Oxidation
Glossy Opaque 8.99 0.33 : 0.67 Glazy Admin
Red Brown Tenmoku, Tenmoku Gold Δ6 Matte 8.65 0.42 : 0.58 Glazy Admin
Peacock Blue Δ6 Semi-matte 8.39 0.18 : 0.82 Glazy Admin
Heino Turquoise ^10 (variation) Δ10 Satin-matte Opaque 4.95 0.53 : 0.47 Glazy Admin
Alligator Raku Δ05½ - 04 Raku
Opaque 25.06 0.09 : 0.91 Glazy Admin
Val Cushing Shino Gustin Rev. Δ9 - 10 Reduction
Glossy 3.97 0.94 : 0.06 Glazy Admin
Reeves Green Δ10 Oxidation
Reduction
Glossy 6.63 0.44 : 0.56 Glazy Admin
VIVIKA'S MAJOLICA HITEMP.tamucc Δ10 Reduction
Glossy 10.4 0.31 : 0.69 Glazy Admin