Terry Rorison, 64 recipes

Name Temp. Atmospheres Surface Transparency Si:Al R20:RO Author Rating
Hansen Clear GA12 Cone 6 Lt. Blue Δ6 Oxidation
Satin Translucent 9.75 0.21 : 0.79 Terry Rorison
Blue Spruce Cone 6 Sugar Maples Δ6 Oxidation
Satin Opaque 8.63 0.2 : 0.8 Terry Rorison
CC Blue Semi-Gloss Cone 6 Δ6 Oxidation
Glossy Opaque 8.93 0.22 : 0.78 Terry Rorison
Ron Roy Black Glossy Cone 6 Δ6 Oxidation
Glossy Opaque 10.55 0.34 : 0.66 Terry Rorison
Brilliant Shiny Cobalt Blue Cone 6 GA24 Δ6 Oxidation
Satin Translucent 8.15 0.28 : 0.72 Terry Rorison
Waterfall Brown Δ6 Oxidation
Satin Opaque 13.18 0.32 : 0.68 Terry Rorison
Pete Pinnell Green Black Δ6 Oxidation
Semi-matte Opaque 4.6 0.5 : 0.5 Terry Rorison
DJ's Perfect Purple Δ6 Oxidation
Semi-matte Opaque 5.59 0.2 : 0.8 Terry Rorison
Red Orange Δ6 Oxidation
Semi-matte Opaque 9.18 0.3 : 0.7 Terry Rorison
Carmen's Turquoise Δ6 Oxidation
Satin Opaque 4.68 0.32 : 0.68 Terry Rorison
Hansen Clear GA12 Darker Green Δ6 Oxidation
Glossy Transparent 9.58 0.21 : 0.79 Terry Rorison
Oribe Green Sugar Maples Δ6 Oxidation
Glossy Semi-opaque 8.64 0.13 : 0.87 Terry Rorison
Blue Green Sugar Maples Δ6 Oxidation
Glossy Transparent 9.06 0.24 : 0.76 Terry Rorison
Ron Roy Zinc Semi-matte Sea Green Δ6 Oxidation
Semi-matte Opaque 8.98 0.24 : 0.76 Terry Rorison
Ron Roy Spearmint Δ6 Oxidation
Glossy Translucent 6.94 0.1 : 0.9 Terry Rorison
Ron Roy High Calcium Semimatte Base 2 Δ6 Oxidation
Semi-matte Translucent 6.94 0.1 : 0.9 Terry Rorison
Blue Green/Copper Red Δ6 Oxidation
Satin Translucent 8.69 0.25 : 0.75 Terry Rorison
Jen's Juicy Fruit Variation (Red Matte) Δ6 Oxidation
Matte Opaque 5.25 0.65 : 0.35 Terry Rorison
Jen's Juicy Fruit Variation (Red Matte) Δ6 Oxidation
Matte Opaque 5.25 0.65 : 0.35 Terry Rorison
Blue-Green Matt Δ6 Oxidation
Matte Opaque 5.16 0.21 : 0.79 Terry Rorison
Transparent Dark Green Glossy Cone 6 Δ6 Oxidation
Glossy Translucent 6.26 0.24 : 0.76 Terry Rorison
Blue Hare's Fur Cone 6 Δ6 Oxidation
Glossy Translucent 6.82 0.44 : 0.56 Terry Rorison
Turquoise Matt Cone 6 Δ6 Oxidation
Matte Opaque 5.12 0.53 : 0.47 Terry Rorison
Satin Matt Cone 6 Rusty Bronze GA23 Δ6 Oxidation
Satin Translucent 5.21 0.52 : 0.48 Terry Rorison
Satin Matt Cone 6 Lt. Blue-Green GA23 Δ6 Oxidation
Satin Translucent 5.21 0.52 : 0.48 Terry Rorison
Satin Matt Cone 6 Lt. Green GA23 Δ6 Oxidation
Satin Translucent 5.21 0.52 : 0.48 Terry Rorison
Hansen Clear GA12 Cone 6 Mottled blue Δ6 Oxidation
Satin Translucent 9.75 0.21 : 0.79 Terry Rorison
Faux Celadon Cone 6 Sugar Maples Δ6 Oxidation
Satin Translucent 11.08 0.28 : 0.72 Terry Rorison
Nutmeg Shino Cone 6 Sugar Maples Δ6 Oxidation
Satin Opaque 7.05 0.22 : 0.78 Terry Rorison
Gloria's Dark Green Cone 6 Sugar Maples Δ6 Oxidation
Glossy Semi-opaque 7.53 0.15 : 0.85 Terry Rorison
Temmoku Sugar Maples Cone 6 Δ6 Oxidation
Glossy Semi-opaque 8.95 0.27 : 0.73 Terry Rorison
GA 20 Cone 6 Lewings SC40E Blue Δ6 Oxidation
Glossy Transparent 11.8 0.24 : 0.76 Terry Rorison
GA 20 Cone 6 Lewings SC40E Red Δ6 Oxidation
Glossy Transparent 11.8 0.24 : 0.76 Terry Rorison
GA 20 Cone 6 Lewings SC40E Blue Gray Δ6 Oxidation
Glossy Transparent 11.8 0.24 : 0.76 Terry Rorison
GA 8 Cone 6 Green Breaking Ochre Δ6 Oxidation
Glossy Transparent 8.72 0.21 : 0.79 Terry Rorison
GA 5 Cone 6 Straw Δ6 Oxidation
Glossy Transparent 10.95 0.25 : 0.75 Terry Rorison
Transparent - T12 C/6 Almost Black Δ6 Oxidation
Glossy Transparent 8.94 0.4 : 0.6 Terry Rorison
Transparent - T12 C/6 Reddish Tan Δ6 Oxidation
Glossy Transparent 8.94 0.4 : 0.6 Terry Rorison
Transparent - T12 C/6 Tan Δ6 Oxidation
Glossy Transparent 8.94 0.4 : 0.6 Terry Rorison
Transparent - T12 C/6 Reddish Brown Δ6 Oxidation
Glossy Transparent 8.94 0.4 : 0.6 Terry Rorison